Product Details:
Type | Corrosion Resistant |
Packaging Size | 50 kg |
Brand | Zeochem |
Packaging Type | Bag |
Country of Origin | Made in India |
Usage | Industrial |
We are the leading manufacturer of Sulphur Mortar from Ahmedabad, India, which is used in Acid Resitant Lining work
Other Details:
Preparation of Mortar:
The mortar should be heated at low tempreture in a suitable kettle by stirring with metal rod or ladle.
The surface shall be laid first with membrane.
Over the dry coat of membrane, the chemical resistant bricks or tiles be placed on spacer chips.
Melted sulphur mortar shall bepoured through joints of bricks or tiles.
In case of vertical surface joints of bricks or tiles are covered by applying with adhesive paper.
Sulphur mortar is poured between the wall surface and the tile or bricks.
Please ensure that no water shall be spilled over the bricks lining works before it completely cured.
Surface Preparation:
The cement plastered surface shall be slightly rough in line level, dry clean, free from dust, dirt, grease, oil etc., maintaining required slope can be adjusted or altered in acid proof lining works.
Mechanical/Physical Properties:
Density of cured mortar: 2.10-2.20g/cc
Bond strength: 10 kg/cm2
Compressive strength: 280 kg/cm2
Flexural strength: 70 kg/cm2
Water absorption: 1%
Note:
If sulphur is over heated or ignited, a tight cover or wet gunny bags shall be kept ready for use in case of fire.
Sulphur mortar burns with a low blue flame.
If this should happen, heating should be stopped and the vessel should be covered with lid or wet gunny bags.
If the mortar thickness or over heating, it should be allowed to cool and stir till it become thin.
Care should be taken that water or damp mortar should not fall in the heating vessel in order to avoid foaming.
Storage Life:
12 months at the temperature 270 deg C